Ryton vs. Torlon Machining
Comparison of Ryton and Torlon Property Values
Ryton |
0.02 |
5,000 |
1,000,000 |
2.5 |
385 |
Material |
---|
Water Absorption Rating |
Tensile Strength |
Flexural Modulus |
Coefficient of Linear Thermal Expansion |
Dielectric Strength |
Torlon 4203 Electrical Grade | Torlon 4301 Bearing Grade | Torlon 5530 Glass Filled |
0.4 | 0.4 | 0.3 |
18,000 | 12,000 | 15,000 |
-- | -- | -- |
1.7 | 1.4 | 2.6 |
580 | -- | 700 |
Material Properties
- Excellent chemical resistance
- Almost no moisture absorption
- Machines to tight tolerances
- Inert to steam, strong bases, fuels and acids
- Very low coefficient of linear thermal expansion
- Inherently flame retardant
- Dimensional stability
- High mechanical strength
- High strength-to-weight ratio
- High dimensional stability
- Low creep
- High thermal endurance
- Machinability
Click here to submit a Request for Quote
Or call us today at 714.579.7700