G-10 vs. G-3 Machining
Comparison of G-10 and G-3 Property Values
G-10 |
0.1 |
45,000 |
2,700 |
0.66 |
-- |
Material |
---|
Water Absorption Rating |
Tensile Strength |
Flexural Modulus |
Coefficient of Linear Thermal Expansion |
Dielectric Strength |
G-3 |
2.65 |
42,000 |
1,800 |
1 |
-- |
Material Properties
- Excellent electrical characteristics
- Superior physical properties
- Machinability
- Excellent flexural, compressive, and impact strengths
- Low moisture absorption
- High dimensional stability
- Machinability