G-9 vs. Nylatron Machining
Comparison of G-9 and Nylatron Property Values
G-9 |
0.6 |
61,600 |
2,000 |
1 |
-- |
Material |
---|
Water Absorption Rating |
Tensile Strength |
Flexural Modulus |
Coefficient of Linear Thermal Expansion |
Dielectric Strength |
Extruded Nylon | Cast Nylon |
1.2 | 0.6 - .12 |
12,400 | 10,000 - 13,500 |
410,000 | 420,000 - 500,000 |
4.5 | 5 |
-- | -- |