Delrin vs. G-7 Machining
Comparison of Delrin and G-7 Property Values
Acetal Homopolymer | Acetal Copolymer |
0.25 | 0.2 |
10,000 | 9,800 |
420 | 370,000 |
6.8 | 6.1 |
-- | -- |
Material |
---|
Water Absorption Rating |
Tensile Strength |
Flexural Modulus |
Coefficient of Linear Thermal Expansion |
Dielectric Strength |
G-7 |
0.1 |
20,000 |
1,600 |
0.9 |
-- |
Material Properties
- Low moisture absorption
- High mechanical strength and rigidity
- Machinability
- Excellent heat and arc resistance
- Good electrical properties under humid conditions
- Machinability